Typically, I used the 2% thoriated for alum and steel. Machine: Miller Econtig (15 yr. old unit).What TIG electrode is best for:Aluminum:Mild Steel:Stainless Steel:If you could choose just 1 electrode for the rest of your life, what would it be?THX
Reply:2% lantanated
Reply:Same here.
Reply:Ditto on 2% Lanthanated for AC work. I get them from HTP Usaweld.2% thorium on all DC work.Weld like a "WELDOR", not a wel-"DERR" MillerDynasty700DX,Dynasty350DX4ea,Dynasty200DX,Li ncolnSW200-2ea.,MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig2ea,MigMax1ea.
Reply:thanks guys. whats the deal with 2% Ceriated(SP?)
Reply:So far, 1.5% or 2%La. But I see a very close performance/resemblence with Diamond Ground's TriMix tungsten, as well as HTP's Quad-Mix tungsten. All are very good so far, but I have yet to push them with high current. 1st on WeldingWeb to have a scrolling sig! HTP Invertig 400HTP Invertig 221HTP ProPulse 300HTP ProPulse 200 x2HTP ProPulse 220MTSHTP Inverarc 200TLP HTP Microcut 875SC
Reply:USA Weld has some good deals on tungsten, so Ive seen. The filler is a little more spendy if you buy from them.
Reply:Originally Posted by bbscampthanks guys. whats the deal with 2% Ceriated(SP?) |
|