Sub-Arc Welding 1/4" wall at 40" a minute

[复制链接]

9万

主题

9万

帖子

29万

积分

论坛元老

Rank: 8Rank: 8

积分
293221
发表于 2021-9-1 00:44:23 | 显示全部楼层 |阅读模式
I need assistance on coming up with a procedure, wire size, amperage and voltage on being able to run without getting pinholes or burning through. I need to keep the speed around 40- 47 inches per minute. The thickness we are running is 1/4" wall. We are running D/C 480 Amps on the inside and 27 Volts and D/C 600 and 31 Volts on the outside, we are running 47-48 inches per minute now. The issue is piholes at this rate, if we turn the heat up to get rid of the piholes we burn through. We have 1 5/16" stickout on the ID welder at these settings. OD welder seams to be dooing just fine, all of the trouble is coming from the ID weld.
Reply:You need an on site consultant for this, which apparently is some form of code work;with the end application use subject to codes---whether you realize this or not.There's all manner of variables and unknowns that need to beobserved, first hand, to get your process established, the results inspectedand certified and tested to show repeatability of the WPS.Since you're the shop manager, it's time to establish in writingexactly what your goal is, then search, recruit, interview, contract, delegate and manage.Blackbird
回复

使用道具 举报

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

Archiver|小黑屋|DiscuzX

GMT+8, 2025-12-20 19:08 , Processed in 0.095531 second(s), 21 queries .

Powered by Discuz! X3.4

Copyright © 2001-2021, Tencent Cloud.

快速回复 返回顶部 返回列表