It says set in 4 to 6 hrs and then overnight above 40 F. I dont have a sheet for it I wonder how much temp accelerates it, both set and cure.. I just put a second gob on, dont believe I disturbed the set, in a while I want to flip and pot another gob on the other side. I am going to put in front of a register. Will it fully cure in 12 hrs at 100 degrees?Last edited by Sberry; 03-22-2022 at 06:06 PM.www.urkafarms.com
Reply:Yes . .
Reply:Yes. Should be rock hard in that time and temp
Reply:Yes it should be good 2 go in 12 hours. If it's real cold when using it, I sometimes heat up the puddle with a heatgun while you are mixing it. it help it flow nice.Miller 211Hypertherm PM 451961 Lincoln Idealarc 250HTP 221 True Wisdom only comes from Pain.
Reply:It something that I had to remove with torch. It has a great smell when torch is used a skunk has a better smell 😉. Dave
Originally Posted by Sberry
It says set in 4 to 6 hrs and then overnight above 40 F. I dont have a sheet for it I wonder how much temp accelerates it, both set and cure.. I just put a second gob on, dont believe I disturbed the set, in a while I want to flip and pot another gob on the other side. I am going to put in front of a register. Will it fully cure in 12 hrs at 100 degrees?
Reply:
Originally Posted by smithdoor
It something that I had to remove with torch. It has a great smell when torch is used a skunk has a better smell