Hi guys.I just saw something on ebay called dynaflow silver braze. I am trying to fill some imperfections on a rough brass casting so it can be chromed.I have been advised to use hard silver solder.From what I read about dynaflow,I don't see why this shouldn't work just as well.Anyone familiar with it and can confirm it will be ok? All input is greatly appeciated!Best regards,Grandpa Marc
Reply:That is the same as Sil-phos. It has a higher melting temp than that of higher silver bearing fillers. It does work wonders for tig brazing tough joints but I don't think it would flow like you need without porosity.Weld like a "WELDOR", not a wel-"DERR" MillerDynasty700DX,Dynasty350DX4ea,Dynasty200DX,Li  ncolnSW200-2ea.,MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig2ea,MigMax1ea.
Reply:Where are you located?Weld like a "WELDOR", not a wel-"DERR" MillerDynasty700DX,Dynasty350DX4ea,Dynasty200DX,Li  ncolnSW200-2ea.,MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig2ea,MigMax1ea.
回复

使用道具 举报

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

Archiver|小黑屋|DiscuzX

GMT+8, 2025-12-26 04:18 , Processed in 0.095054 second(s), 18 queries .

Powered by Discuz! X3.4

Copyright © 2001-2021, Tencent Cloud.

快速回复 返回顶部 返回列表