my company uses L56 wire of lincoln .I=260-310A,U=28-32V, there are tawny things appeared after welding .my opinion they are SIO2 or others oxide .if dont grind it ,then the weld bead cant pass ut,so i want to ask what is it ? how to appear?
Reply:showz us pikters so weez cans seen watt the 'ell eeu are talk 'bout. (Spell check and Google translate are your friend also). "Hey I didn't come to look and learn, I came to turn and burn.... If I can't light up, I'm gonna light out!"-JodyIdealarc 250 "Fatman"MM 252MM 211 "Little boy" Victor Torches
Reply:It's the copperLast edited by Burpee; 02-14-2014 at 06:31 AM.Bubble gumTooth pixDuct tapeBlack glueGBMF hammerScrew gun --bad battery (see above) |
|