Didnt think i dipped. Its a touch start and seems to stick alot Attached Images
Reply:After resharpening Attached Images
Reply:What's your post flow at? How many amps u using?maybe to much stick out
Reply:Couple welds about 80 amps 18 on the argon Attached Images
Reply:Any tips are welcome
Reply:I thought we were talking about ur tungsten? What tungsten are u using and what size?
Reply:1/16 i think friendbgave it to me
Reply:How about the other questions I asked you. Do u know what post flow is and stick out?
Reply:I try and pull away slowly for post flow andstick out is like 3/8 i guess.
Reply:U pry have to much stick out and not enough post flow. Try the changes and see what happens. Your tungsten should look like it did when u grinded it. 18 cfh sounds like plenty tho. I use even less. Do u know how many seconds of post flow you had it set at?
Reply:Cheap welder no post flow.
Reply:Then u pry have a gas valve on the torch. U need to leave it on for about 5 sec minimum if ur welding at 80 amp. At 180 ill leave it in for about 15 sec. A rule of thumb is u want  about 1 second post flow for every 10 amps but I can't afford to do that until I start getting paid more often to weld for poeple.
回复

使用道具 举报

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

Archiver|小黑屋|DiscuzX

GMT+8, 2026-1-2 06:55 , Processed in 0.147077 second(s), 20 queries .

Powered by Discuz! X3.4

Copyright © 2001-2021, Tencent Cloud.

快速回复 返回顶部 返回列表